CFR767-3


The combination of processing cycles in high temperature environments combined with aggressive fluxes can cause degradation of standard Durostone grades.

The solution is Durostone CFR767, which is specially formulated for aggressive fluxes and high temperature process configurations.

The resin used to produce Durostone CFR767 can withstand temperatures up to 300°C. When the solder bath temperature exceeds 265°C and the bottom PCB preheat exceeds 140°C, Durostone CFR767 should be used instead of the standard grade.

Durostone CFR767 has excellent flux resistance. When fluxes containing halides or dicarboxylic acids are used in high-volume production, the lifetime of standard grade materials is reduced, so Durostone CFR767 is the ideal solution.

Taros Kami

Author:

Ms. Tina

Phone/WhatsApp:

8618680371609

Produk populér
News parusahaan
Exhibition News
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

You may also like
Related Categories

Email pikeun supplier ieu

taluk:
Hapé:
email:
pesen:

Your message must be betwwen 20-8000 characters

Taros Kami

Author:

Ms. Tina

Phone/WhatsApp:

8618680371609

Produk populér
News parusahaan
Exhibition News
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

Kami bakal ngahubungi anjeun langsung

Eusian langkung seueur inpormasi supados tiasa nyambung sareng anjeun gancang

Pernyataan privasi: Privasi anjeun penting pisan pikeun kami. Perusahaan urang jangji henteu ngungkabkeun inpormasi pribadi anjeun kana ijin anu jelas.

Ngirim